Basic steps for good brazing
STEP N° 3 SETTING OF THE PARTS
The clean parts, covered in flux, must be correctly positioned to be brazed.
Remember that the capillary action is possible when the separation between the faces is clearly defined.
SOLDARGEN 100
ARGENTA SP - 2
ARGENTA SP - 5
ARGENTA SP - 6
ARGENTA SP - 15 |
|
0,03 - 0,12MM. |
- For these brazing filler metals the recommended separation for joints with an overlap more than 25mm long is 0.17 - 0.38mm.
- The gap or clearance recommended for joints not considering the overlapping length is from 0.05 mm to 0.12 mm using the following filler metal with over 25% of silver content;
ARGENTA 30 FC
ARGENTA 34 FC
ARGENTA 40 FC
ARGENTA 45 FC
ARGENTA 50 FC
ARGENTA 56 FC |
|
0,05 - 0,12mm. |
|
ARGENTA 2560
ARGENTA 3060
ARGENTA 35-2S
ARGENTA 4060
ARGENTA 456
ARGENTA 506 |